6.02007	0.588565
8.02676	0.504484
10.0334	0.588565
12.0401	0.840807
14.0468	0.840807
16.0535	0.840807
18.0602	1.09305
20.0669	1.59753
22.0736	1.68161
24.0803	1.93386
26.087	2.10202
28.0936	2.27018
30.1003	2.27018
32.107	2.6065
34.1137	2.77466
36.1204	2.85874
38.1271	3.44731
40.1338	3.53139
42.1405	3.69955
44.1472	3.78363
46.1538	4.3722
48.1605	4.54036
50.1672	4.62444
52.1739	5.12892
54.1806	5.213
56.1873	5.71749
58.194	5.88565
60.2007	6.05381
62.2074	6.64238
64.214	6.72646
66.2207	7.23094
68.2274	7.31502
70.2341	7.81951
72.2408	7.98767
74.2475	8.15583
76.2542	8.32399
78.2609	8.40807
80.2676	8.91256
82.2742	9.08072
84.2809	9.5852
86.2876	9.66928
88.2943	10.1738
90.301	10.426
92.3077	10.5101
94.3144	10.9305
96.3211	11.0987
98.3278	11.6031
100.334	11.6872
102.341	12.2758
104.348	12.7803
106.355	12.8643
108.361	13.0325
110.368	13.2007
112.375	13.4529
114.381	13.537
116.388	13.7052
118.395	14.2096
120.401	14.3778
122.408	14.546
124.415	14.7141
126.421	15.2186
128.428	15.3027
130.435	15.7231
132.441	16.0594
134.448	16.0594
136.455	16.5639
138.462	16.7321
140.468	16.9843
142.475	16.9843
144.482	17.2365
146.488	17.4047
148.495	17.5729
150.502	17.741
152.508	17.9092
154.515	18.4137
156.522	18.4137
158.528	18.75
160.535	18.9182
162.542	19.0863
164.548	19.2545
166.555	19.4226
168.562	19.5908
170.569	19.5908
172.575	19.9271
174.582	20.0953
176.589	20.2635
178.595	20.4316
180.602	20.5998
182.609	20.7679
184.615	20.7679
186.622	21.1043
188.629	21.2724
190.635	21.4406
192.642	21.7769
194.649	21.861
196.656	22.2814
198.662	22.1973
200.669	22.4496
202.676	22.5336
204.682	22.6177
206.689	22.7859
208.696	22.954
210.702	23.0381
212.709	23.2063
214.716	23.4585
216.722	23.7108
218.729	23.7948
220.736	24.0471
222.742	24.2152
224.749	24.2152
226.756	24.2152
228.763	24.2993
230.769	24.2993
232.776	24.2993
234.783	24.5516
236.789	24.5516
238.796	24.6357
240.803	24.8038
242.809	25.0561
244.816	25.0561
246.823	25.3083
248.829	25.3924
250.836	25.3924
252.843	25.4765
254.849	25.5605
256.856	25.7287
258.863	25.7287
260.87	25.8128
262.876	25.8969
264.883	25.9809
266.89	26.065
268.896	26.1491
270.903	26.4854
272.91	26.4854
274.916	26.4854
276.923	26.5695
278.93	26.5695
280.936	26.6536
282.943	26.7377
284.95	26.9058
286.957	26.9899
288.963	27.074
290.97	27.3262
292.977	27.4103
294.983	27.4944
296.99	27.5785
298.997	27.6626
301.003	27.7466
303.01	27.8307
305.017	28.083
307.023	28.083
309.03	28.083
311.037	28.083
313.043	28.167
315.05	28.3352
317.057	28.3352
319.064	28.3352
321.07	28.3352
323.077	28.3352
325.084	28.5874
327.09	28.6715
329.097	28.6715
331.104	28.6715
333.11	28.7556
335.117	28.9238
337.124	29.0078
339.13	29.0078
341.137	29.0078
343.144	29.0078
345.151	29.0919
347.157	29.2601
349.164	29.2601
351.171	29.2601
353.177	29.2601
355.184	29.2601
357.191	29.5123
359.197	29.5964
361.204	29.7646
363.211	29.8487
365.217	29.8487
367.224	29.8487
369.231	29.9327
371.237	30.1009
373.244	30.185
375.251	30.185
377.258	30.185
379.264	30.185
381.271	30.3531
383.278	30.4372
385.284	30.4372
387.291	30.4372
389.298	30.4372
391.304	30.6054
393.311	30.6895
395.318	30.6895
397.324	30.6895
399.331	30.6895
401.338	30.6895
403.344	30.6895
405.351	30.6895
407.358	30.6895
409.365	30.6895
411.371	30.6895
413.378	30.6895
415.385	30.6895
417.391	30.6895
419.398	30.6895
421.405	30.7735
423.411	30.9417
425.418	31.0258
427.425	31.0258
429.431	31.0258
431.438	31.1099
433.445	31.278
435.452	31.3621
437.458	31.3621
439.465	31.3621
441.472	31.3621
443.478	31.3621
445.485	31.3621
447.492	31.3621
449.498	31.3621
451.505	31.3621
453.512	31.3621
455.518	31.3621
457.525	31.4462
459.532	31.6143
461.538	31.6143
463.545	31.6143
465.552	31.6143
467.559	31.6143
469.565	31.8666
471.572	31.8666
473.579	31.8666
475.585	31.8666
477.592	31.8666
479.599	31.8666
481.605	31.8666
483.612	31.8666
485.619	31.8666
487.625	31.8666
489.632	31.8666
491.639	31.8666
493.645	31.8666
495.652	31.8666
497.659	31.8666
499.666	31.9507
501.672	32.1188
503.679	32.2029
505.686	32.2029
507.692	32.2029
509.699	32.4552
511.706	32.5392
513.712	32.5392
515.719	32.5392
517.726	32.5392
519.732	32.5392
521.739	32.5392
523.746	32.5392
525.753	32.5392
527.759	32.5392
529.766	32.5392
531.773	32.5392
533.779	32.5392
535.786	32.5392
537.793	32.5392
539.799	32.5392
541.806	32.6233
543.813	32.7915
545.819	32.7915
547.826	32.7915
549.833	32.7915
551.839	32.9596
553.846	33.0437
555.853	33.0437
557.86	33.0437
559.866	33.0437
561.873	33.0437
563.88	33.0437
565.886	33.0437
567.893	33.0437
569.9	33.0437
571.906	33.0437
573.913	33.0437
575.92	33.0437
577.926	33.0437
579.933	33.0437
581.94	33.0437
583.946	33.0437
585.953	33.0437
587.96	33.0437
589.967	33.1278
591.973	33.296
593.98	33.38
595.987	33.38
597.993	33.38
600	33.4641
602.007	33.6323
604.013	33.7164
606.02	33.7164
608.027	33.7164
610.033	33.7164
612.04	33.8845
614.047	33.9686
616.054	33.9686
618.06	33.9686
620.067	33.9686
622.074	34.1368
624.08	34.2209
626.087	34.2209
628.094	34.2209
630.1	34.2209
632.107	34.3049
634.114	34.4731
636.12	34.5572
638.127	34.5572
640.134	34.5572
642.14	34.6413
644.147	34.8094
646.154	34.8935
648.161	34.8935
650.167	34.8935
652.174	34.8935
654.181	34.8935
656.187	34.8935
658.194	34.8935
660.201	34.9776
662.207	35.1457
664.214	35.1457
666.221	35.1457
668.227	35.1457
670.234	35.1457
672.241	35.398
674.247	35.398
676.254	35.398
678.261	35.398
680.268	35.4821
682.274	35.6502
684.281	35.7343
686.288	35.7343
688.294	35.7343
690.301	35.7343
692.308	35.9865
694.314	35.9865
696.321	35.9865
698.328	35.9865
700.334	35.9865
702.341	36.0706
704.348	36.2388
706.355	36.2388
708.361	36.2388
710.368	36.2388
712.375	36.3229
714.381	36.5751
716.388	36.5751
718.395	36.5751
720.401	36.5751
722.408	36.6592
724.415	36.8274
726.421	36.9114
728.428	36.9114
730.435	36.9114
732.441	36.9114
734.448	37.1637
736.455	37.1637
738.462	37.1637
740.468	37.1637
742.475	37.1637
744.482	37.2478
746.488	37.4159
748.495	37.4159
750.502	37.5
752.508	37.6682
754.515	37.8363
756.522	38.0886
758.528	38.0886
760.535	38.0886
762.542	38.3408
764.548	38.3408
766.555	38.3408
768.562	38.3408
770.569	38.3408
772.575	38.4249
774.582	38.593
776.589	38.593
778.595	38.593
780.602	38.593
782.609	38.8453
784.615	38.9294
786.622	39.0135
788.629	39.1816
790.635	39.2657
792.642	39.2657
794.649	39.4339
796.656	39.7702
798.662	39.7702
800.669	39.7702
802.676	39.8543
804.682	40.0224
806.689	40.1065
808.696	40.1065
810.702	40.1065
812.709	40.1065
814.716	40.1906
816.722	40.4428
818.729	40.4428
820.736	40.4428
822.742	40.611
824.749	40.9473
826.756	40.9473
828.763	41.0314
830.769	41.3677
832.776	41.5359
834.783	41.62
836.789	41.62
838.796	41.7881
840.803	41.8722
842.809	41.9563
844.816	42.1244
846.823	42.1244
848.829	42.2085
850.836	42.4608
852.843	42.713
854.849	42.7971
856.856	42.7971
858.863	42.8812
860.87	43.0493
862.876	43.0493
864.883	43.3016
866.89	43.3016
868.896	43.3016
870.903	43.3857
872.91	43.722
874.916	43.8901
876.923	43.9742
878.93	44.2265
880.936	44.3946
882.943	44.4787
884.95	44.7309
886.957	44.8991
888.963	45.0673
890.97	45.1513
892.977	45.1513
894.983	45.3195
896.99	45.4036
898.997	45.5717
901.003	45.6558
903.01	45.6558
905.017	45.7399
907.023	46.3285
909.03	46.4966
911.037	46.5807
913.043	46.833
915.05	47.0011
917.057	47.1693
919.064	47.1693
921.07	47.5056
923.077	47.926
925.084	48.0101
927.09	48.2623
929.097	48.4305
931.104	48.5987
933.11	48.6827
935.117	49.1872
937.124	49.3554
939.13	49.4395
941.137	49.6917
943.144	49.8599
945.151	50.028
947.157	50.1962
949.164	50.7007
951.171	51.2052
953.177	51.2892
955.184	51.5415
957.191	51.6256
959.197	51.7937
961.204	51.8778
963.211	52.4664
965.217	52.8868
967.224	53.0549
969.231	53.5594
971.237	53.6435
973.244	53.8117
975.251	53.9798
977.258	54.4843
979.264	54.9888
981.271	55.157
983.278	55.5774
985.284	55.6614
987.291	56.1659
989.298	56.3341
991.304	56.8386
993.311	57.343
995.318	57.5112
997.324	58.5202
999.331	58.6043
1001.34	59.1928
1003.34	59.2769
1005.35	59.7814
1007.36	60.2859
1009.36	60.454
1011.37	62.3879
1013.38	62.472
1015.38	63.565
1017.39	63.6491
1019.4	68.2735
1021.4	68.778
1023.41	68.8621
1025.42	73.1502
1027.42	73.3184
1029.43	75.3363
1031.44	75.2522
1033.44	74.7478
1035.45	75.6627
1037.46	75.5539
1039.46	67.9238
1041.47	67.8733
1043.48	67.341
1045.48	67.1669
1047.49	66.8624
1049.5	53.1198
1051.51	49.4395
1053.51	48.935
1055.52	48.8509
1057.53	47.4215
1059.53	47.3374
1061.54	46.917
1063.55	46.2444
1065.55	46.2444
1067.56	46.0762
1069.57	45.4877
1071.57	45.4036
1073.58	45.3195
1075.59	44.815
1077.59	44.3105
1079.6	44.1424
1081.61	43.9742
1083.61	43.6379
1085.62	43.6379
1087.63	43.6379
1089.63	43.5538
1091.64	43.0493
1093.65	43.0493
1095.65	42.8812
1097.66	42.7971
1099.67	42.7971
1101.67	42.713
1103.68	42.3767
1105.69	42.2085
1107.69	42.1244
1109.7	42.1244
1111.71	41.9563
1113.71	41.8722
1115.72	41.7881
1117.73	41.62
1119.73	41.62
1121.74	41.62
1123.75	41.62
1125.75	41.3677
1127.76	41.2836
1129.77	41.1996
1131.77	40.9473
1133.78	40.9473
1135.79	40.9473
1137.79	40.9473
1139.8	40.7791
1141.81	40.6951
1143.81	40.6951
1145.82	40.6951
1147.83	40.6951
1149.83	40.6951
1151.84	40.6951
1153.85	40.6951
1155.85	40.6951
1157.86	40.6951
1159.87	40.6951
1161.87	40.6951
1163.88	40.6951
1165.89	40.6951
1167.89	40.6951
1169.9	40.6951
1171.91	40.4428
1173.91	40.4428
1175.92	40.5269
1177.93	40.4428
1179.93	40.3587
1181.94	40.1906
1183.95	40.1065
1185.95	40.1065
1187.96	40.1065
1189.97	40.1065
1191.97	40.1065
1193.98	40.1065
1195.99	40.1065
1197.99	40.1065
1200	40.1065
1202.01	40.1065
1204.01	40.1065
1206.02	40.1065
1208.03	40.1065
1210.03	40.1065
1212.04	40.1065
1214.05	40.1065
1216.05	40.1065
1218.06	40.1065
1220.07	40.1065
1222.07	40.1065
1224.08	40.1065
1226.09	40.1065
1228.09	40.1065
1230.1	40.1065
1232.11	40.1065
1234.11	40.1065
1236.12	40.1065
1238.13	40.1065
1240.13	40.1065
1242.14	40.1065
1244.15	40.1065
1246.15	40.1065
1248.16	40.0224
1250.17	39.8543
1252.17	39.7702
1254.18	39.7702
1256.19	39.7702
1258.19	39.6861
1260.2	39.5179
1262.21	39.5179
1264.21	39.5179
1266.22	39.5179
1268.23	39.5179
1270.23	39.5179
1272.24	39.5179
1274.25	39.5179
1276.25	39.5179
1278.26	39.5179
1280.27	39.5179
1282.27	39.5179
1284.28	39.5179
1286.29	39.5179
1288.29	39.5179
1290.3	39.5179
1292.31	39.5179
1294.31	39.5179
1296.32	39.5179
1298.33	39.5179
1300.33	39.5179
1302.34	39.5179
1304.35	39.5179
1306.35	39.5179
1308.36	39.5179
1310.37	39.5179
1312.37	39.5179
1314.38	39.5179
1316.39	39.5179
1318.39	39.5179
1320.4	39.5179
1322.41	39.5179
1324.41	39.5179
1326.42	39.5179
1328.43	39.5179
1330.43	39.5179
1332.44	39.5179
1334.45	39.5179
1336.45	39.5179
1338.46	39.5179
1340.47	39.5179
1342.47	39.5179
1344.48	39.5179
1346.49	39.5179
1348.49	39.5179
1350.5	39.5179
1352.51	39.5179
1354.52	39.5179
1356.52	39.5179
1358.53	39.5179
1360.54	39.602
1362.54	39.7702
1364.55	39.7702
1366.56	39.7702
1368.56	39.7702
1370.57	40.0224
1372.58	40.1065
1374.58	40.1065
1376.59	40.1065
1378.6	40.1065
1380.6	40.1065
1382.61	40.1065
1384.62	40.1065
1386.62	40.1065
1388.63	40.1065
1390.64	40.1065
1392.64	40.1065
1394.65	40.1065
1396.66	40.1065
1398.66	40.1065
1400.67	40.1065
1402.68	40.1065
1404.68	40.1065
1406.69	40.1065
1408.7	40.1065
1410.7	40.1065
1412.71	40.1065
1414.72	40.1065
1416.72	40.1065
1418.73	40.1065
1420.74	40.1065
1422.74	40.1065
1424.75	40.1065
1426.76	40.1065
1428.76	40.1065
1430.77	40.1065
1432.78	40.1065
1434.78	40.1065
1436.79	40.1065
1438.8	40.1065
1440.8	40.1065
1442.81	40.1065
1444.82	40.1065
1446.82	40.1065
1448.83	40.1065
1450.84	40.1065
1452.84	40.1065
1454.85	40.1065
1456.86	40.1065
1458.86	40.1065
1460.87	40.1065
1462.88	40.1065
1464.88	40.1065
1466.89	40.1065
1468.9	40.1065
1470.9	40.1065
1472.91	40.3587
1474.92	40.4428
1476.92	40.4428
1478.93	40.4428
1480.94	40.4428
1482.94	40.6951
1484.95	40.6951
1486.96	40.6951
1488.96	40.6951
1490.97	40.6951
1492.98	40.6951
1494.98	40.6951
1496.99	40.6951
1499	40.6951
1501	40.6951
1503.01	40.6951
1505.02	40.6951
1507.02	40.6951
1509.03	40.6951
1511.04	40.6951
1513.04	40.6951
1515.05	40.6951
1517.06	40.6951
1519.06	40.6951
1521.07	40.7791
1523.08	40.9473
1525.08	40.9473
1527.09	40.9473
1529.1	40.9473
1531.1	41.0314
1533.11	41.1996
1535.12	41.2836
1537.12	41.2836
1539.13	41.2836
1541.14	41.2836
1543.14	41.2836
1545.15	41.2836
1547.16	41.2836
1549.16	41.2836
1551.17	41.2836
1553.18	41.2836
1555.18	41.2836
1557.19	41.2836
1559.2	41.2836
1561.2	41.2836
1563.21	41.2836
1565.22	41.2836
1567.22	41.2836
1569.23	41.2836
1571.24	41.2836
1573.24	41.2836
1575.25	41.2836
1577.26	41.2836
1579.26	41.2836
1581.27	41.2836
1583.28	41.2836
1585.28	41.2836
1587.29	41.2836
1589.3	41.2836
1591.3	41.2836
1593.31	41.2836
1595.32	41.2836
1597.32	41.2836
1599.33	41.2836
1601.34	41.2836
1603.34	41.2836
1605.35	41.3677
1607.36	41.5359
1609.36	41.62
1611.37	41.62
1613.38	41.62
1615.38	41.704
1617.39	41.8722
1619.4	41.8722
1621.4	41.8722
1623.41	41.8722
1625.42	41.8722
1627.42	41.8722
1629.43	41.8722
1631.44	41.8722
1633.44	41.8722
1635.45	41.8722
1637.46	41.8722
1639.46	41.8722
1641.47	41.8722
1643.48	41.8722
1645.48	41.8722
1647.49	41.8722
1649.5	41.8722
1651.51	41.8722
1653.51	41.8722
1655.52	42.0404
1657.53	42.1244
1659.53	42.1244
1661.54	42.1244
1663.55	42.2085
1665.55	42.3767
1667.56	42.5448
1669.57	42.5448
1671.57	42.5448
1673.58	42.5448
1675.59	42.4608
1677.59	42.5448
1679.6	42.5448
1681.61	42.4608
1683.61	42.4608
1685.62	42.4608
1687.63	42.4608
1689.63	42.4608
1691.64	42.4608
1693.65	42.4608
1695.65	42.4608
1697.66	42.4608
1699.67	42.4608
1701.67	42.4608
1703.68	42.4608
1705.69	42.4608
1707.69	42.4608
1709.7	42.4608
1711.71	42.4608
1713.71	42.4608
1715.72	42.4608
1717.73	42.4608
1719.73	42.4608
1721.74	42.4608
1723.75	42.4608
1725.75	42.4608
1727.76	42.4608
1729.77	42.4608
1731.77	42.5448
1733.78	42.7971
1735.79	42.7971
1737.79	42.7971
1739.8	42.7971
1741.81	42.9652
1743.81	43.0493
1745.82	43.0493
1747.83	43.0493
1749.83	43.0493
1751.84	43.0493
1753.85	43.0493
1755.85	43.0493
1757.86	43.0493
1759.87	43.0493
1761.87	43.0493
1763.88	43.0493
1765.89	43.0493
1767.89	43.0493
1769.9	43.0493
1771.91	43.0493
1773.91	43.0493
1775.92	43.0493
1777.93	43.0493
1779.93	43.0493
1781.94	43.0493
1783.95	43.0493
1785.95	43.0493
1787.96	43.0493
1789.97	43.0493
1791.97	43.0493
1793.98	43.0493
1795.99	43.0493
1797.99	43.0493
1800	42.9652
1802.01	43.1334
1804.01	43.0493
1806.02	43.0493
1808.03	43.0493
1810.03	43.0493